87 Concrete building blocks made with recycled
It was therefore necessary to investigate the effect of varying the percentage of fine fraction replacement for a mix that already had either 60% or 20% of the coarse fraction replaced with RCA and RMA aggregate 16 shows that the detrimental effect of increasing fine fraction replacement on the 20% coarse RMA mix is similar to the